Abstract

The development of environmentally friendly materials has been the focus of many research groups in recent years due to increased harmful effects of plastics on the environment. Bio-based materials are considered a key solution from a sustainable manufacturing perspective. The nano-coating of biopolymer blends with silver nanoparticles is the subject of challenging research projects in line with the EU Directive on environment protection and sustainable manufacturing. Coating biopolymers with silver nanoparticles provides an antimicrobial and antiviral active surface. In this work, we develop silver nanoparticle-coated biopolymer Arboblend V2 Nature pellets. The main goal is to obtain a new material with antibacterial action obtained from the blending of a biopolymer pellets with silver nanoparticles through physical vapor deposition. The study is divided in three steps. The first step represents the silver nano-coating of the Arboblend V2 Nature and the characterization of the coated/raw pellets. The second step involves the injection molding of the silver nano-coated pellets and the characterization of the samples obtained. The last step regards the press molding of the coated pellets in order to obtain thin films, as well as their characterization. The PVD-sputtering technique is used to coat the pellets with silver nanoparticles. This process is especially optimized for coating raw materials with high water content and small-size pellets. The mechanical properties, surface chemical composition and the thermal properties of the both virgin and silver nanoparticle-coated biopolymer pellets are measured and analyzed for mechanical and thermal resistance of the nano-coating layer. Differential scanning calorimetry, scanning electron microscopy, X-ray photoemission spectroscopy and nanoindentation mechanical testing is performed. The calorimetry test detects no significant alteration of the biopolymer produced from the PVD process and confirms the optimized PVD process for nano-coating of the Arboblend V2 Nature pellets with a viable application in nano-silver–biopolymer composite products.

Original languageEnglish
Article number7706
Number of pages14
JournalApplied Sciences (Switzerland)
Volume11
Issue number16
DOIs
Publication statusPublished - Aug 2021
Externally publishedYes

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 9 - Industry, Innovation, and Infrastructure
    SDG 9 Industry, Innovation, and Infrastructure

Keywords

  • Biopolymer
  • Characterization
  • Coating
  • Pellets
  • Silver

Fingerprint

Dive into the research topics of 'Xps, sem, dsc and nanoindentation characterization of silver nanoparticle-coated biopolymer pellets'. Together they form a unique fingerprint.

Cite this