Skip to main navigation Skip to search Skip to main content

Reactive magnetron-sputtered ZrN, ZrO, and ZrON monolayers and ZrO/ZrN multilayers for hydrophobic and tribomechanically enhanced nanostructured coatings

  • Linda Aissani
  • , Ahlam Belgroune
  • , Ahcene Keziz
  • , Abdelhak Ayad
  • , Sara Fares
  • , Akram Alhussein
  • , Taha Abdel Mohaymen Taha
  • , Ali Alsalme
  • , Mikhael Bechelany
  • , Altaf Hussain
  • , Ahmed Barhoum

Research output: Contribution to journal › Article › peer-review

Abstract

Surface degradation under mechanical and tribological stresses is strongly influenced by coating composition, microstructure, and environmental conditions. Despite advances in nanostructured coatings, the synergistic mechanisms governing their mechanical and wear performance remain insufficiently understood. In this study, ZrN, ZrO, ZrON monolayers, and ZrO/ZrN multilayer coatings were deposited on Ti6Al4V via reactive magnetron sputtering to investigate the effects of composition on microstructure, mechanical properties, and tribological performance. The study demonstrated that the successful formation of cubic ZrN and monoclinic ZrO2 phases was confirmed through X-ray diffraction and Raman spectroscopy techniques. Beneficially, the multilayer deposition effectively reduced the grain size from (18-12.7) nm in monolayers to 7.2 nm among the deposited multilayers. Energy Dispersive Spectroscopy analysis indicated controlled incorporation of nitrogen (48 at. %) and oxygen (51 at. %) in the respective coatings. Measurements of the contact angle between the film surface and the water droplet showed that the surface hydrophobicity increased with increasing roughness of the coatings. Nanoindentation measurements showed hardness values of 21.1 ± 0.5 GPa (ZrN), 25.0 ± 0.5 GPa (ZrO), 32.1 ± 0.5 GPa (ZrON), and 28.1 ± 1.2 GPa (ZrO/ZrN multilayer), respectively. The multilayer also exhibited high resistance to plastic deformation (H/E = 0.084; H3/E2 = 0.198 GPa), with recorded friction coefficients of 0.52 (ZrN), 0.46 (ZrO), and 0.33 (ZrO/ZrN multilayer) at 3 N. Additionally, oxygen-containing layers developed compact tribo-oxidized films. Residual stress analysis indicated compressive ZrO (−461 MPa) partially offsetting tensile ZrN (+1099 MPa), stabilizing the coatings. The multilayer achieved the lowest wear rate (1.7×10−7mm3/Nm), nearly an order of magnitude lower than monolayers. The findings demonstrate that interface engineering and multilayer structures in Zr-N, and Zr-O-based coatings improve load-bearing capacity and offer hardness and wear resistance, thereby effectively reducing friction, and fatigue in harsh applications.

Original languageEnglish
Pages (from-to)2847-2862
Number of pages16
JournalJournal of Materials Research and Technology
Volume45
DOIs
Publication statusPublished - 1 Nov 2026

Keywords

  • Nanoindentation
  • Reactive magnetron sputtering
  • Residual stress
  • Wear resistance
  • Zirconium oxynitride
  • Zirconium-based coatings

Fingerprint

Dive into the research topics of 'Reactive magnetron-sputtered ZrN, ZrO, and ZrON monolayers and ZrO/ZrN multilayers for hydrophobic and tribomechanically enhanced nanostructured coatings'. Together they form a unique fingerprint.

Cite this